Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (39) Inactive Alloys (3) U.S. EPA Registered Antimicrobial (30) You Searched For: rockwell-b-scale:[70 TO 80] tensile-strength:[60 TO 70] rockwell-f-scale:[60 TO 70] CLEAR this search X SAVE this search << Page 1 >> 42 Alloys Found Alloy UNS#DesignationActiveView C15500 * Yes C15500 Profile Suppliers of C15500 C16500 * Yes C16500 Profile Suppliers of C16500 C21000 * Gilding, 95% Yes C21000 Profile Suppliers of C21000 C22000 * Commercial Bronze, 90% Yes C22000 Profile Suppliers of C22000 C22600 * Jewelry Bronze, 87-1/2% Yes C22600 Profile Suppliers of C22600 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C33200 High Leaded Brass (Tube) Yes C33200 Profile Suppliers of C33200 C33500 Low-Leaded Brass Yes C33500 Profile Suppliers of C33500 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C34200 High Leaded Brass, 64-1/2% Yes C34200 Profile Suppliers of C34200 C35000 Medium Leaded Brass, 62% Yes C35000 Profile Suppliers of C35000 C35300 High Leaded Brass, 62% Yes C35300 Profile Suppliers of C35300 C35600 Extra High Leaded Brass Yes C35600 Profile Suppliers of C35600 C36000 Free-Cutting Brass Yes C36000 Profile Suppliers of C36000 C36010 Leaded Brass (Free-Cutting Brass) Yes C36010 Profile Suppliers of C36010 C36200 Leaded Brass No C36200 Profile Suppliers of C36200 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C40800 * Silicon Brass No C40800 Profile Suppliers of C40800 C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C41500 * Tin Brass Yes C41500 Profile Suppliers of C41500 C42200 * Yes C42200 Profile Suppliers of C42200 C42500 * Yes C42500 Profile Suppliers of C42500 C43000 * Tin Brass Yes C43000 Profile Suppliers of C43000 C43400 * Yes C43400 Profile Suppliers of C43400 C43500 * Tin Brass Yes C43500 Profile Suppliers of C43500 C50500 * Phosphor Bronze, 1.25% E Yes C50500 Profile Suppliers of C50500 C51100 * Yes C51100 Profile Suppliers of C51100 C54400 Phosphor Bronze B-2 Yes C54400 Profile Suppliers of C54400 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C70400 * Copper-Nickel, 5% Yes C70400 Profile Suppliers of C70400 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C75400 Nickel Silver, 65-15 Yes C75400 Profile Suppliers of C75400 C75700 * Nickel Silver, 65-12 Yes C75700 Profile Suppliers of C75700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>