4 Alloys Found

Alloy UNS#DesignationActiveView

C86700

Yes C86700 Profile
Suppliers of C86700

C87850 *

Copper Silicon Alloy Yes C87850 Profile
Suppliers of C87850

C87900

Copper Silicon Yes C87900 Profile
Suppliers of C87900

C99750

Yes C99750 Profile
Suppliers of C99750