Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (6) You Searched For: rockwell-b-scale:[70 TO 80] modulus-of-elasticity-in-tension:[19000 TO 20000] CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C18135 Yes C18135 Profile Suppliers of C18135 C71000 * Copper-Nickel, 20% Yes C71000 Profile Suppliers of C71000 C72500 * Yes C72500 Profile Suppliers of C72500 C82200 * Copper Beryllium 3C Yes C82200 Profile Suppliers of C82200 C82600 * Copper Beryllium 245C Yes C82600 Profile Suppliers of C82600 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>