Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (29) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (24) You Searched For: rockwell-b-scale:[80 TO 90] tensile-strength:[100 TO 110] element_names:"Lead" CLEAR this search X SAVE this search << Page 1 >> 31 Alloys Found Alloy UNS#DesignationActiveView C19000 * Yes C19000 Profile Suppliers of C19000 C19100 Yes C19100 Profile Suppliers of C19100 C23000 * Red Brass, 85% Yes C23000 Profile Suppliers of C23000 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51100 * Yes C51100 Profile Suppliers of C51100 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C53400 Phosphor Bronze B-1 Yes C53400 Profile Suppliers of C53400 C63200 * Aluminum Bronze Yes C63200 Profile Suppliers of C63200 C63800 * Yes C63800 Profile Suppliers of C63800 C64200 * Aluminum Bronze Yes C64200 Profile Suppliers of C64200 C64400 * Aluminum Bronze No C64400 Profile Suppliers of C64400 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C65400 Yes C65400 Profile Suppliers of C65400 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C66900 * Manganese Brass Yes C66900 Profile Suppliers of C66900 C68800 * Yes C68800 Profile Suppliers of C68800 C69000 * Copper Zinc No C69000 Profile Suppliers of C69000 C69300 * ECO Brass Yes C69300 Profile Suppliers of C69300 C69400 Silicon Red Brass Yes C69400 Profile Suppliers of C69400 C69410 Yes C69410 Profile Suppliers of C69410 C69430 Yes C69430 Profile Suppliers of C69430 C69710 Yes C69710 Profile Suppliers of C69710 C72500 * Yes C72500 Profile Suppliers of C72500 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C75200 * Nickel Silver, 65-18 Yes C75200 Profile Suppliers of C75200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>