Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (19) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (16) You Searched For: rockwell-b-scale:[90 TO 100] rockwell-30t-scale:[60 TO 65] CLEAR this search X SAVE this search << Page 1 >> 20 Alloys Found Alloy UNS#DesignationActiveView C17300 Copper Beryllium Yes C17300 Profile Suppliers of C17300 C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C41500 * Tin Brass Yes C41500 Profile Suppliers of C41500 C43000 * Tin Brass Yes C43000 Profile Suppliers of C43000 C51100 * Yes C51100 Profile Suppliers of C51100 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C66900 * Manganese Brass Yes C66900 Profile Suppliers of C66900 C72500 * Yes C72500 Profile Suppliers of C72500 C75400 Nickel Silver, 65-15 Yes C75400 Profile Suppliers of C75400 C75700 * Nickel Silver, 65-12 Yes C75700 Profile Suppliers of C75700 C78200 Yes C78200 Profile Suppliers of C78200 C78270 Nickel Silver (Nickel Silver) Yes C78270 Profile Suppliers of C78270 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>