Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (20) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (17) You Searched For: seam-weld:"Good" elongation:[15 TO 18] CLEAR this search X SAVE this search << Page 1 >> 20 Alloys Found Alloy UNS#DesignationActiveView C19500 * Yes C19500 Profile Suppliers of C19500 C49355 * Copper Zinc Bismuth Alloy Yes C49355 Profile Suppliers of C49355 C62400 * Aluminum Bronze,11% Yes C62400 Profile Suppliers of C62400 C63000 * Aluminum Bronze Yes C63000 Profile Suppliers of C63000 C64770 * Yes C64770 Profile Suppliers of C64770 C65100 * Low-Silicon Bronze B Yes C65100 Profile Suppliers of C65100 C67420 Yes C67420 Profile Suppliers of C67420 C68370 Yes C68370 Profile Suppliers of C68370 C69300 * ECO Brass Yes C69300 Profile Suppliers of C69300 C69310 * SnEco Yes C69310 Profile Suppliers of C69310 C69350 Yes C69350 Profile Suppliers of C69350 C70400 * Copper-Nickel, 5% Yes C70400 Profile Suppliers of C70400 C70600 * Copper-Nickel, 10% Yes C70600 Profile Suppliers of C70600 C72500 * Yes C72500 Profile Suppliers of C72500 C87500 * Coppe Silicon Alloy Yes C87500 Profile Suppliers of C87500 C87600 * Copper Silcon Alloy Yes C87600 Profile Suppliers of C87600 C87800 * Cast Silicon Bronze Yes C87800 Profile Suppliers of C87800 C87850 * Copper Silicon Alloy Yes C87850 Profile Suppliers of C87850 C87860 * Yes C87860 Profile Suppliers of C87860 C89720 * Copper-Bismuth Alloy (TECO) Yes C89720 Profile Suppliers of C89720 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>