Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (5) You Searched For: soldering:"Fair" coated-metal-arc-welding:"Good" CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C61000 * Yes C61000 Profile Suppliers of C61000 C61800 * Yes C61800 Profile Suppliers of C61800 C61900 * Yes C61900 Profile Suppliers of C61900 C63200 * Aluminum Bronze Yes C63200 Profile Suppliers of C63200 C66930 * Copper-Manganese Alloy Yes C66930 Profile Suppliers of C66930 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>