Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (25) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (22) You Searched For: tensile-strength:[120 TO 130] brazing:"Excellent" CLEAR this search X SAVE this search << Page 1 >> 26 Alloys Found Alloy UNS#DesignationActiveView C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26000 * Cartridge Brass, 70% Yes C26000 Profile Suppliers of C26000 C26100 * Brass No C26100 Profile Suppliers of C26100 C26130 * Yes C26130 Profile Suppliers of C26130 C26200 * Yes C26200 Profile Suppliers of C26200 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C42600 * Yes C42600 Profile Suppliers of C42600 C44730 Yes C44730 Profile Suppliers of C44730 C44750 * Tin Brass Yes C44750 Profile Suppliers of C44750 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51980 * Yes C51980 Profile Suppliers of C51980 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C52180 * Yes C52180 Profile Suppliers of C52180 C52400 * Phospher Bronze 10% D Yes C52400 Profile Suppliers of C52400 C52480 * Yes C52480 Profile Suppliers of C52480 C64751 Yes C64751 Profile Suppliers of C64751 C64752 Yes C64752 Profile Suppliers of C64752 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 C66913 * Copper-Zinc-Manganese Yes C66913 Profile Suppliers of C66913 C66915 * Copper-Zinc-Manganese Yes C66915 Profile Suppliers of C66915 C70318 Yes C70318 Profile Suppliers of C70318 C72500 * Yes C72500 Profile Suppliers of C72500 C72900 * Yes C72900 Profile Suppliers of C72900 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C96600 * Yes C96600 Profile Suppliers of C96600 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>