Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
14 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C19050 * |
SPKFC-5E (High Copper) | Yes |
C19050 Profile Suppliers of C19050 |
C44750 * |
Tin Brass | Yes |
C44750 Profile Suppliers of C44750 |
C52100 * |
Phospher Bronze, 8% C | Yes |
C52100 Profile Suppliers of C52100 |
C52180 * |
Yes |
C52180 Profile Suppliers of C52180 |
|
C52480 * |
Yes |
C52480 Profile Suppliers of C52480 |
|
C53800 |
Yes |
C53800 Profile Suppliers of C53800 |
|
C61500 * |
Yes |
C61500 Profile Suppliers of C61500 |
|
C64400 * |
Aluminum Bronze | No |
C64400 Profile Suppliers of C64400 |
C64727 * |
Copper Silicon Alloy (MAX375) | Yes |
C64727 Profile Suppliers of C64727 |
C64728 * |
Copper-Nickel-Zinc-Silicon Alloy | Yes |
C64728 Profile Suppliers of C64728 |
C66930 * |
Copper-Manganese Alloy | Yes |
C66930 Profile Suppliers of C66930 |
C70330 |
Yes |
C70330 Profile Suppliers of C70330 |
|
C70350 * |
Yes |
C70350 Profile Suppliers of C70350 |
|
C72670 |
Yes |
C72670 Profile Suppliers of C72670 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |