Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
15 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C15000 * |
Zirconium Copper | Yes |
C15000 Profile Suppliers of C15000 |
C15150 * |
Yes |
C15150 Profile Suppliers of C15150 |
|
C24000 * |
Low Brass, 80% | Yes |
C24000 Profile Suppliers of C24000 |
C28330 * |
Low-Lead Yellow Brass | Yes |
C28330 Profile Suppliers of C28330 |
C51000 * |
Phosphor Bronze, 5% A | Yes |
C51000 Profile Suppliers of C51000 |
C51100 * |
Yes |
C51100 Profile Suppliers of C51100 |
|
C51180 * |
Yes |
C51180 Profile Suppliers of C51180 |
|
C53400 |
Phosphor Bronze B-1 | Yes |
C53400 Profile Suppliers of C53400 |
C65500 * |
High-Silicon Bronze A | Yes |
C65500 Profile Suppliers of C65500 |
C72660 * |
Yes |
C72660 Profile Suppliers of C72660 |
|
C76200 |
Nickel Silver | Yes |
C76200 Profile Suppliers of C76200 |
C78200 |
Yes |
C78200 Profile Suppliers of C78200 |
|
C78270 |
Nickel Silver (Nickel Silver) | Yes |
C78270 Profile Suppliers of C78270 |
C82000 * |
Copper Beryllium 10C | Yes |
C82000 Profile Suppliers of C82000 |
C95600 * |
Yes |
C95600 Profile Suppliers of C95600 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |