Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (129) Inactive Alloys (10) U.S. EPA Registered Antimicrobial (78) You Searched For: yield-strength:[10 TO 30] elongation:[15 TO 18] CLEAR this search X SAVE this search << Page 1 2 3 >> 139 Alloys Found Alloy UNS#DesignationActiveView C10100 * Oxygen-Free-Electronic (OFE) Yes C10100 Profile Suppliers of C10100 C10200 * Oxygen-Free (OF) Yes C10200 Profile Suppliers of C10200 C10300 * Oxygen-Free Copper (OFXLP) Yes C10300 Profile Suppliers of C10300 C10400 * Oxygen-Free with Ag (OFS) Yes C10400 Profile Suppliers of C10400 C10500 * Oxygen-Free with Ag (OFS) Yes C10500 Profile Suppliers of C10500 C10700 * Oxygen-Free with Ag (OFS) Yes C10700 Profile Suppliers of C10700 C10800 * Yes C10800 Profile Suppliers of C10800 C11300 * Tough Pitch with Ag (STP) Yes C11300 Profile Suppliers of C11300 C11400 * Tough Pitch with Ag (STP) Yes C11400 Profile Suppliers of C11400 C11500 * Tough Pitch with Ag (STP) Yes C11500 Profile Suppliers of C11500 C11600 * Tough Pitch with Ag (STP) Yes C11600 Profile Suppliers of C11600 C12000 * Phosphorus-Deoxidized, Low Residual P (DLP) Yes C12000 Profile Suppliers of C12000 C12100 * Phosphorus-Deoxidized, Low Residual P (DLPS) Yes C12100 Profile Suppliers of C12100 C12500 * Fire-Refined Tough Pitch (FRTP) Yes C12500 Profile Suppliers of C12500 C12510 * Yes C12510 Profile Suppliers of C12510 C12700 * Copper Alloy No C12700 Profile Suppliers of C12700 C12800 * Copper Alloy No C12800 Profile Suppliers of C12800 C12900 * Fire-Refined Tough Pitch with Ag (FRSTP) Yes C12900 Profile Suppliers of C12900 C13000 Copper Alloy No C13000 Profile Suppliers of C13000 C14500 * Tellurium-Bearing (PTE) Yes C14500 Profile Suppliers of C14500 C14510 * Tellurium-Bearing Yes C14510 Profile Suppliers of C14510 C14520 * Phosphorus-Deoxidized,Tellurium-Bearing (DPTE) Yes C14520 Profile Suppliers of C14520 C14530 * Yes C14530 Profile Suppliers of C14530 C14700 * Sulfur-Bearing Yes C14700 Profile Suppliers of C14700 C14710 * Copper Alloy No C14710 Profile Suppliers of C14710 C14720 Copper Alloy No C14720 Profile Suppliers of C14720 C16500 * Yes C16500 Profile Suppliers of C16500 C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C17300 Copper Beryllium Yes C17300 Profile Suppliers of C17300 C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C18135 Yes C18135 Profile Suppliers of C18135 C18200 Chromium Copper Yes C18200 Profile Suppliers of C18200 C18400 Chromium Copper Yes C18400 Profile Suppliers of C18400 C18500 High Copper No C18500 Profile Suppliers of C18500 C18700 Free-Machining Cu Yes C18700 Profile Suppliers of C18700 C19000 * Yes C19000 Profile Suppliers of C19000 C19100 Yes C19100 Profile Suppliers of C19100 C19200 * Yes C19200 Profile Suppliers of C19200 C19400 * Yes C19400 Profile Suppliers of C19400 C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C26800 * Yellow Brass, 66% Yes C26800 Profile Suppliers of C26800 C27000 * Yellow Brass, 65% Yes C27000 Profile Suppliers of C27000 C28330 * Low-Lead Yellow Brass Yes C28330 Profile Suppliers of C28330 C31400 Leaded Commercial Bronze Yes C31400 Profile Suppliers of C31400 C31600 Leaded Commercial Bronze (Nickel-Bearing) Yes C31600 Profile Suppliers of C31600 C32000 Leaded Red Brass Yes C32000 Profile Suppliers of C32000 C33500 Low-Leaded Brass Yes C33500 Profile Suppliers of C33500 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C34500 Yes C34500 Profile Suppliers of C34500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 2 3 >>