Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (3) You Searched For: yield-strength:[10 TO 30] yield-strength:[130 TO 150] CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C17300 Copper Beryllium Yes C17300 Profile Suppliers of C17300 C53800 Yes C53800 Profile Suppliers of C53800 C61500 * Yes C61500 Profile Suppliers of C61500 C82500 * Copper Beryllium 20C Yes C82500 Profile Suppliers of C82500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>