Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (3) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (2) You Searched For: yield-strength:[110 TO 130] melting-point-solidus:[1900 TO 1950] element_names:"Lead" CLEAR this search X SAVE this search << Page 1 >> 3 Alloys Found Alloy UNS#DesignationActiveView C61900 * Yes C61900 Profile Suppliers of C61900 C70252 * Copper Nickel (NKC 388) Yes C70252 Profile Suppliers of C70252 C70390 Yes C70390 Profile Suppliers of C70390 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>