Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
15 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C81500 |
Chrome Copper | Yes |
C81500 Profile Suppliers of C81500 |
C86100 |
Manganese Bronze | Yes |
C86100 Profile Suppliers of C86100 |
C86200 |
Yes |
C86200 Profile Suppliers of C86200 |
|
C86700 |
Yes |
C86700 Profile Suppliers of C86700 |
|
C95200 * |
Yes |
C95200 Profile Suppliers of C95200 |
|
C95300 * |
Yes |
C95300 Profile Suppliers of C95300 |
|
C95400 * |
Yes |
C95400 Profile Suppliers of C95400 |
|
C95500 * |
Yes |
C95500 Profile Suppliers of C95500 |
|
C95600 * |
Yes |
C95600 Profile Suppliers of C95600 |
|
C95700 * |
Yes |
C95700 Profile Suppliers of C95700 |
|
C95800 * |
Yes |
C95800 Profile Suppliers of C95800 |
|
C96400 * |
70-30 Copper Nickel | Yes |
C96400 Profile Suppliers of C96400 |
C96600 * |
Yes |
C96600 Profile Suppliers of C96600 |
|
C99400 * |
Non-Dezincificztion Alloy | Yes |
C99400 Profile Suppliers of C99400 |
C99500 * |
Special Alloys | Yes |
C99500 Profile Suppliers of C99500 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |