Alloy UNS# | Designation | Active | View |
---|---|---|---|
C31400 |
Leaded Commercial Bronze | Yes |
C31400 Profile Suppliers of C31400 |
C31600 |
Leaded Commercial Bronze (Nickel-Bearing) | Yes |
C31600 Profile Suppliers of C31600 |
C32000 |
Leaded Red Brass | Yes |
C32000 Profile Suppliers of C32000 |
C51900 * |
Yes |
C51900 Profile Suppliers of C51900 |
|
C52100 * |
Phospher Bronze, 8% C | Yes |
C52100 Profile Suppliers of C52100 |
C74500 * |
Nickel Silver, 65-10 | Yes |
C74500 Profile Suppliers of C74500 |
C75700 * |
Nickel Silver, 65-12 | Yes |
C75700 Profile Suppliers of C75700 |
C76200 |
Nickel Silver | Yes |
C76200 Profile Suppliers of C76200 |
C78200 |
Yes |
C78200 Profile Suppliers of C78200 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |