Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
13 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C26100 * |
Brass | No |
C26100 Profile Suppliers of C26100 |
C26130 * |
Yes |
C26130 Profile Suppliers of C26130 |
|
C26200 * |
Yes |
C26200 Profile Suppliers of C26200 |
|
C26800 * |
Yellow Brass, 66% | Yes |
C26800 Profile Suppliers of C26800 |
C27000 * |
Yellow Brass, 65% | Yes |
C27000 Profile Suppliers of C27000 |
C28000 * |
Muntz Metal, 60% | Yes |
C28000 Profile Suppliers of C28000 |
C33000 |
Low Leaded Brass (Tube) | Yes |
C33000 Profile Suppliers of C33000 |
C33100 |
Leaded Brass | No |
C33100 Profile Suppliers of C33100 |
C33200 |
High Leaded Brass (Tube) | Yes |
C33200 Profile Suppliers of C33200 |
C33500 |
Low-Leaded Brass | Yes |
C33500 Profile Suppliers of C33500 |
C51900 * |
Yes |
C51900 Profile Suppliers of C51900 |
|
C54400 |
Phosphor Bronze B-2 | Yes |
C54400 Profile Suppliers of C54400 |
C94700 * |
Cast Nickel-Tin Bronze | Yes |
C94700 Profile Suppliers of C94700 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |