Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (4) You Searched For: yield-strength:[70 TO 90] capacity-for-being-cold-worked:"Good" elongation:[39 TO 42] CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C50725 * Yes C50725 Profile Suppliers of C50725 C52100 * Phospher Bronze, 8% C Yes C52100 Profile Suppliers of C52100 C70600 * Copper-Nickel, 10% Yes C70600 Profile Suppliers of C70600 C71000 * Copper-Nickel, 20% Yes C71000 Profile Suppliers of C71000 C77000 Nickel Silver, 55-18 Yes C77000 Profile Suppliers of C77000 C78200 Yes C78200 Profile Suppliers of C78200 C78270 Nickel Silver (Nickel Silver) Yes C78270 Profile Suppliers of C78270 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>