Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (4) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (4) You Searched For: yield-strength:[70 TO 90] rockwell-30t-scale:[25 TO 30] tensile-strength:[100 TO 110] CLEAR this search X SAVE this search << Page 1 >> 4 Alloys Found Alloy UNS#DesignationActiveView C41100 * Tin Brass Yes C41100 Profile Suppliers of C41100 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>