Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (18) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (14) You Searched For: yield-strength:[90 TO 110] electrical-conductivity:[30.0 TO 35.0] CLEAR this search X SAVE this search << Page 1 >> 18 Alloys Found Alloy UNS#DesignationActiveView C19027 * NB 115 (High Copper) Yes C19027 Profile Suppliers of C19027 C19040 * CAC5 (High Copper) Yes C19040 Profile Suppliers of C19040 C19050 * SPKFC-5E (High Copper) Yes C19050 Profile Suppliers of C19050 C19250 * SPKFC-5W (High Copper) Yes C19250 Profile Suppliers of C19250 C40810 * Yes C40810 Profile Suppliers of C40810 C40820 * Yes C40820 Profile Suppliers of C40820 C40850 * Yes C40850 Profile Suppliers of C40850 C40860 * Yes C40860 Profile Suppliers of C40860 C42220 * Yes C42220 Profile Suppliers of C42220 C42230 Yes C42230 Profile Suppliers of C42230 C42300 Yes C42300 Profile Suppliers of C42300 C42520 * Yes C42520 Profile Suppliers of C42520 C50725 * Yes C50725 Profile Suppliers of C50725 C50780 * Yes C50780 Profile Suppliers of C50780 C64740 * Yes C64740 Profile Suppliers of C64740 C64751 Yes C64751 Profile Suppliers of C64751 C64752 Yes C64752 Profile Suppliers of C64752 C70290 * Yes C70290 Profile Suppliers of C70290 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>