Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (35) Inactive Alloys (4) U.S. EPA Registered Antimicrobial (29) You Searched For: yield-strength:[90 TO 110] yield-strength:[110 TO 130] CLEAR this search X SAVE this search << Page 1 >> 39 Alloys Found Alloy UNS#DesignationActiveView C17000 * Copper Beryllium Yes C17000 Profile Suppliers of C17000 C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C17300 Copper Beryllium Yes C17300 Profile Suppliers of C17300 C17400 * Beryllium Copper No C17400 Profile Suppliers of C17400 C17410 * Copper Beryllium Yes C17410 Profile Suppliers of C17410 C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C17530 * Copper Beryllium Yes C17530 Profile Suppliers of C17530 C19050 * SPKFC-5E (High Copper) Yes C19050 Profile Suppliers of C19050 C19250 * SPKFC-5W (High Copper) Yes C19250 Profile Suppliers of C19250 C42600 * Yes C42600 Profile Suppliers of C42600 C44250 * Yes C44250 Profile Suppliers of C44250 C44730 Yes C44730 Profile Suppliers of C44730 C51080 * Yes C51080 Profile Suppliers of C51080 C51180 * Yes C51180 Profile Suppliers of C51180 C51980 * Yes C51980 Profile Suppliers of C51980 C52180 * Yes C52180 Profile Suppliers of C52180 C52480 * Yes C52480 Profile Suppliers of C52480 C61900 * Yes C61900 Profile Suppliers of C61900 C63800 * Yes C63800 Profile Suppliers of C63800 C64400 * Aluminum Bronze No C64400 Profile Suppliers of C64400 C64728 * Copper-Nickel-Zinc-Silicon Alloy Yes C64728 Profile Suppliers of C64728 C64751 Yes C64751 Profile Suppliers of C64751 C64752 Yes C64752 Profile Suppliers of C64752 C64770 * Yes C64770 Profile Suppliers of C64770 C64780 * Yes C64780 Profile Suppliers of C64780 C64790 Yes C64790 Profile Suppliers of C64790 C64810 NKC4820 Yes C64810 Profile Suppliers of C64810 C65400 Yes C65400 Profile Suppliers of C65400 C68800 * Yes C68800 Profile Suppliers of C68800 C69000 * Copper Zinc No C69000 Profile Suppliers of C69000 C69750 Yes C69750 Profile Suppliers of C69750 C70330 Yes C70330 Profile Suppliers of C70330 C70350 * Yes C70350 Profile Suppliers of C70350 C70370 * Yes C70370 Profile Suppliers of C70370 C72600 * Copper Nickel No C72600 Profile Suppliers of C72600 C72800 * Yes C72800 Profile Suppliers of C72800 C76200 Nickel Silver Yes C76200 Profile Suppliers of C76200 C82800 * Copper Beryllium 275C Yes C82800 Profile Suppliers of C82800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>