6 Alloys Found

Alloy UNS#DesignationActiveView

C64775

Copper-nickel-silicon Yes C64775 Profile
Suppliers of C64775

C69100 *

Yes C69100 Profile
Suppliers of C69100

C76390

Copper Nickel Zinc No C76390 Profile
Suppliers of C76390

C79350

Yes C79350 Profile
Suppliers of C79350

C89720 *

Copper-Bismuth Alloy (TECO) Yes C89720 Profile
Suppliers of C89720

C90280 *

Yes C90280 Profile
Suppliers of C90280
* signifies an alloy registered with the U.S. EPA as Antimicrobial.