Saved Copper Alloys

Saved Searches

Copper Alloy Advanced Search Help

We'd Love Your Input

Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.

30 Alloys Found

Alloy UNS#DesignationActiveView

C82400 *

Beryllium Copper 165C Yes C82400 Profile
Suppliers of C82400

C82500 *

Beryllium Copper 20C Yes C82500 Profile
Suppliers of C82500

C82600 *

Beryllium Copper 245C Yes C82600 Profile
Suppliers of C82600

C82700 *

High Copper Alloy Yes C82700 Profile
Suppliers of C82700

C82800 *

Beryllium Copper 275C Yes C82800 Profile
Suppliers of C82800

C84800

Plumbing Goods Brass Yes C84800 Profile
Suppliers of C84800

C85430

Yes C85430 Profile
Suppliers of C85430

C85800

Yes C85800 Profile
Suppliers of C85800

C87200

Silicon Bronze No C87200 Profile
Suppliers of C87200

C87400

Yes C87400 Profile
Suppliers of C87400

C87500 *

Coppe Silicon Alloy Yes C87500 Profile
Suppliers of C87500

C87600 *

Copper Silcon Alloy Yes C87600 Profile
Suppliers of C87600

C87800 *

Cast Silicon Bronze Yes C87800 Profile
Suppliers of C87800

C87850 *

Copper Silicon Alloy Yes C87850 Profile
Suppliers of C87850

C87900

Copper Silicon Yes C87900 Profile
Suppliers of C87900

C89320 *

Yes C89320 Profile
Suppliers of C89320

C89545

Yes C89545 Profile
Suppliers of C89545

C89838

Yes C89838 Profile
Suppliers of C89838

C89940 *

Yes C89940 Profile
Suppliers of C89940

C91100

Yes C91100 Profile
Suppliers of C91100

C91300

Yes C91300 Profile
Suppliers of C91300

C92800

Yes C92800 Profile
Suppliers of C92800

C93200

Yes C93200 Profile
Suppliers of C93200

C93400

Yes C93400 Profile
Suppliers of C93400

C94700 *

Cast Nickel-Tin Bronze Yes C94700 Profile
Suppliers of C94700

C94800

Yes C94800 Profile
Suppliers of C94800

C97300

Yes C97300 Profile
Suppliers of C97300

C97400

Yes C97400 Profile
Suppliers of C97400

C97600

Yes C97600 Profile
Suppliers of C97600

C97800

Yes C97800 Profile
Suppliers of C97800
* signifies an alloy registered with the U.S. EPA as Antimicrobial.