113 Alloys Found

Alloy UNS#DesignationActiveView

C15000 *

Zirconium Copper Yes C15000 Profile
Suppliers of C15000

C15500 *

Yes C15500 Profile
Suppliers of C15500

C15720 *

Dispersion Strengthned Alloy Yes C15720 Profile
Suppliers of C15720

C15760 *

Dispersion Strengthened Alloy Yes C15760 Profile
Suppliers of C15760

C16200 *

Cadmium Copper Yes C16200 Profile
Suppliers of C16200

C16210 *

High Copper Alloy No C16210 Profile
Suppliers of C16210

C16500 *

Yes C16500 Profile
Suppliers of C16500

C17000 *

Beryllium Copper Yes C17000 Profile
Suppliers of C17000

C17200 *

Beryllium Copper Yes C17200 Profile
Suppliers of C17200

C17500 *

Beryllium Copper Yes C17500 Profile
Suppliers of C17500

C17510 *

Beryllium Copper Yes C17510 Profile
Suppliers of C17510

C18100

Yes C18100 Profile
Suppliers of C18100

C18135

Yes C18135 Profile
Suppliers of C18135

C18150

Yes C18150 Profile
Suppliers of C18150

C18200

Chromium Copper Yes C18200 Profile
Suppliers of C18200

C18400

Chromium Copper Yes C18400 Profile
Suppliers of C18400

C18500

High Copper No C18500 Profile
Suppliers of C18500

C18625 *

HRSC Yes C18625 Profile
Suppliers of C18625

C19000 *

Yes C19000 Profile
Suppliers of C19000

C19100

Yes C19100 Profile
Suppliers of C19100

C19200 *

Yes C19200 Profile
Suppliers of C19200

C19400 *

Yes C19400 Profile
Suppliers of C19400

C21000 *

Gilding, 95% Yes C21000 Profile
Suppliers of C21000

C22000 *

Commercial Bronze, 90% Yes C22000 Profile
Suppliers of C22000

C22600 *

Jewelry Bronze, 87-1/2% Yes C22600 Profile
Suppliers of C22600

C23000 *

Red Brass, 85% Yes C23000 Profile
Suppliers of C23000

C24000 *

Low Brass, 80% Yes C24000 Profile
Suppliers of C24000

C26000 *

Cartridge Brass, 70% Yes C26000 Profile
Suppliers of C26000

C26100 *

Brass No C26100 Profile
Suppliers of C26100

C26130 *

Yes C26130 Profile
Suppliers of C26130

C26200 *

Yes C26200 Profile
Suppliers of C26200

C26800 *

Yellow Brass, 66% Yes C26800 Profile
Suppliers of C26800

C27000 *

Yellow Brass, 65% Yes C27000 Profile
Suppliers of C27000

C27400 *

Yellow Brass, 63% Yes C27400 Profile
Suppliers of C27400

C28000 *

Muntz Metal, 60% Yes C28000 Profile
Suppliers of C28000

C31600

Leaded Commercial Bronze (Nickel-Bearing) Yes C31600 Profile
Suppliers of C31600

C33000

Low Leaded Brass (Tube) Yes C33000 Profile
Suppliers of C33000

C33100

Leaded Brass No C33100 Profile
Suppliers of C33100

C33200

High Leaded Brass (Tube) Yes C33200 Profile
Suppliers of C33200

C33500

Low-Leaded Brass Yes C33500 Profile
Suppliers of C33500

C34000

Medium Leaded Brass, 64-1/2% Yes C34000 Profile
Suppliers of C34000

C34200

High Leaded Brass, 64-1/2% Yes C34200 Profile
Suppliers of C34200

C34500

Yes C34500 Profile
Suppliers of C34500

C35000

Medium Leaded Brass, 62% Yes C35000 Profile
Suppliers of C35000

C35300

High Leaded Brass, 62% Yes C35300 Profile
Suppliers of C35300

C35600

Extra High Leaded Brass Yes C35600 Profile
Suppliers of C35600

C36000

Free-Cutting Brass Yes C36000 Profile
Suppliers of C36000

C36010

Leaded Brass (Free-Cutting Brass) Yes C36010 Profile
Suppliers of C36010

C36200

Leaded Brass No C36200 Profile
Suppliers of C36200

C37000

Free-Cutting Muntz Metal Yes C37000 Profile
Suppliers of C37000
* signifies an alloy registered with the U.S. EPA as Antimicrobial.