Saved Copper Alloys

Saved Searches

Copper Alloy Advanced Search Help

We'd Love Your Input

Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.

14 Alloys Found

Alloy UNS#DesignationActiveView

C17000 *

Beryllium Copper Yes C17000 Profile
Suppliers of C17000

C17200 *

Beryllium Copper Yes C17200 Profile
Suppliers of C17200

C17300

Beryllium Copper Yes C17300 Profile
Suppliers of C17300

C19910 *

NKT 322 (High Copper) Yes C19910 Profile
Suppliers of C19910

C61900 *

Yes C61900 Profile
Suppliers of C61900

C70252 *

Copper Nickel (NKC 388) Yes C70252 Profile
Suppliers of C70252

C72600 *

Copper Nickel No C72600 Profile
Suppliers of C72600

C72700 *

Yes C72700 Profile
Suppliers of C72700

C72800 *

Yes C72800 Profile
Suppliers of C72800

C72900 *

Yes C72900 Profile
Suppliers of C72900

C82400 *

Beryllium Copper 165C Yes C82400 Profile
Suppliers of C82400

C82500 *

Beryllium Copper 20C Yes C82500 Profile
Suppliers of C82500

C82510 *

Beryllium Copper 21C Yes C82510 Profile
Suppliers of C82510

C82700 *

High Copper Alloy Yes C82700 Profile
Suppliers of C82700
* signifies an alloy registered with the U.S. EPA as Antimicrobial.