6 Alloys Found

Alloy UNS#DesignationActiveView

C19040 *

CAC5 (High Copper) Yes C19040 Profile
Suppliers of C19040

C50500 *

Phosphor Bronze, 1.25% E Yes C50500 Profile
Suppliers of C50500

C50580 *

Yes C50580 Profile
Suppliers of C50580

C50780 *

Yes C50780 Profile
Suppliers of C50780

C61500 *

Yes C61500 Profile
Suppliers of C61500

C65100 *

Low-Silicon Bronze B Yes C65100 Profile
Suppliers of C65100
* signifies an alloy registered with the U.S. EPA as Antimicrobial.