49 Alloys Found

Alloy UNS#DesignationActiveView

C21000 *

Gilding, 95% Yes C21000 Profile
Suppliers of C21000

C22000 *

Commercial Bronze, 90% Yes C22000 Profile
Suppliers of C22000

C22600 *

Jewelry Bronze, 87-1/2% Yes C22600 Profile
Suppliers of C22600

C23000 *

Red Brass, 85% Yes C23000 Profile
Suppliers of C23000

C23400 *

Yes C23400 Profile
Suppliers of C23400

C24000 *

Low Brass, 80% Yes C24000 Profile
Suppliers of C24000

C26000 *

Cartridge Brass, 70% Yes C26000 Profile
Suppliers of C26000

C26100 *

Brass No C26100 Profile
Suppliers of C26100

C26130 *

Yes C26130 Profile
Suppliers of C26130

C26200 *

Yes C26200 Profile
Suppliers of C26200

C26800 *

Yellow Brass, 66% Yes C26800 Profile
Suppliers of C26800

C27000 *

Yellow Brass, 65% Yes C27000 Profile
Suppliers of C27000

C27400 *

Yellow Brass, 63% Yes C27400 Profile
Suppliers of C27400

C27450

Yellow Brass Yes C27450 Profile
Suppliers of C27450

C27451

Yellow Brass (Yellow Brass) Yes C27451 Profile
Suppliers of C27451

C27453

Copper Zinc Alloy Yes C27453 Profile
Suppliers of C27453

C27460

Yes C27460 Profile
Suppliers of C27460

C28340

Yes C28340 Profile
Suppliers of C28340

C33000

Low Leaded Brass (Tube) Yes C33000 Profile
Suppliers of C33000

C33100

Leaded Brass No C33100 Profile
Suppliers of C33100

C33200

High Leaded Brass (Tube) Yes C33200 Profile
Suppliers of C33200

C36300

Copper-Zinc-Lead Alloy Yes C36300 Profile
Suppliers of C36300

C40410 *

Copper-Zinc-Tin Alloy Yes C40410 Profile
Suppliers of C40410

C40500 *

Penny Bronze Yes C40500 Profile
Suppliers of C40500

C40800 *

Silicon Brass No C40800 Profile
Suppliers of C40800

C40810 *

Yes C40810 Profile
Suppliers of C40810

C40850 *

Yes C40850 Profile
Suppliers of C40850

C40860 *

Yes C40860 Profile
Suppliers of C40860

C40950 *

Yes C40950 Profile
Suppliers of C40950

C41100 *

Tin Brass Yes C41100 Profile
Suppliers of C41100

C41120 *

Yes C41120 Profile
Suppliers of C41120

C41125 *

Yes C41125 Profile
Suppliers of C41125

C41300 *

Tin Brass Yes C41300 Profile
Suppliers of C41300

C41500 *

Tin Brass Yes C41500 Profile
Suppliers of C41500

C42200 *

Yes C42200 Profile
Suppliers of C42200

C42210 *

Tin Brass Yes C42210 Profile
Suppliers of C42210

C42220 *

Yes C42220 Profile
Suppliers of C42220

C42230

Yes C42230 Profile
Suppliers of C42230

C42300

Yes C42300 Profile
Suppliers of C42300

C42500 *

Yes C42500 Profile
Suppliers of C42500

C42520 *

Yes C42520 Profile
Suppliers of C42520

C42600 *

Yes C42600 Profile
Suppliers of C42600

C43000 *

Tin Brass Yes C43000 Profile
Suppliers of C43000

C43400 *

Yes C43400 Profile
Suppliers of C43400

C43500 *

Tin Brass Yes C43500 Profile
Suppliers of C43500

C44300 *

Admiralty, Arsenical Yes C44300 Profile
Suppliers of C44300

C44400 *

Admiralty, Antimonial Yes C44400 Profile
Suppliers of C44400

C44500 *

Admiralty, Phosphorized Yes C44500 Profile
Suppliers of C44500

C49100

Yes C49100 Profile
Suppliers of C49100
* signifies an alloy registered with the U.S. EPA as Antimicrobial.