28 Alloys Found

Alloy UNS#DesignationActiveView

C15715 *

Dispersion Strengthened Alloy Yes C15715 Profile
Suppliers of C15715

C15720 *

Dispersion Strengthned Alloy Yes C15720 Profile
Suppliers of C15720

C15730 *

Copper Alloy Yes C15730 Profile
Suppliers of C15730

C15750 *

Dispersion Strengthened Copper (C3/60) Yes C15750 Profile
Suppliers of C15750

C15760 *

Dispersion Strengthened Alloy Yes C15760 Profile
Suppliers of C15760

C17000 *

Beryllium Copper Yes C17000 Profile
Suppliers of C17000

C17300

Beryllium Copper Yes C17300 Profile
Suppliers of C17300

C17400 *

Beryllium Copper No C17400 Profile
Suppliers of C17400

C17410 *

Beryllium Copper Yes C17410 Profile
Suppliers of C17410

C17450 *

Beryllium Copper Yes C17450 Profile
Suppliers of C17450

C17455

Beryllium Copper Yes C17455 Profile
Suppliers of C17455

C17460 *

Beryllium Copper Yes C17460 Profile
Suppliers of C17460

C17465

Beryllium Copper Yes C17465 Profile
Suppliers of C17465

C17500 *

Beryllium Copper Yes C17500 Profile
Suppliers of C17500

C17510 *

Beryllium Copper Yes C17510 Profile
Suppliers of C17510

C17530 *

Beryllium Copper Yes C17530 Profile
Suppliers of C17530

C18900 *

Yes C18900 Profile
Suppliers of C18900

C19500 *

Yes C19500 Profile
Suppliers of C19500

C27460

Yes C27460 Profile
Suppliers of C27460

C63600

Yes C63600 Profile
Suppliers of C63600

C63800 *

Yes C63800 Profile
Suppliers of C63800

C68350 *

Low Silicon Brass Yes C68350 Profile
Suppliers of C68350

C68700 *

Aluminum Brass, Arsenical Yes C68700 Profile
Suppliers of C68700

C68800 *

Yes C68800 Profile
Suppliers of C68800

C69000 *

Copper Zinc No C69000 Profile
Suppliers of C69000

C69100 *

Yes C69100 Profile
Suppliers of C69100

C69150 *

Copper Zinc Alloy (Copper Zinc Alloy) Yes C69150 Profile
Suppliers of C69150

C72800 *

Yes C72800 Profile
Suppliers of C72800