Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (36) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (27) You Searched For: capacity-for-being-cold-worked:"Excellent" seam-weld:"Fair" CLEAR this search X SAVE this search << Page 1 >> 37 Alloys Found Alloy UNS#DesignationActiveView C17000 * Beryllium Copper Yes C17000 Profile Suppliers of C17000 C17300 Beryllium Copper Yes C17300 Profile Suppliers of C17300 C17400 * Beryllium Copper No C17400 Profile Suppliers of C17400 C17410 * Beryllium Copper Yes C17410 Profile Suppliers of C17410 C17450 * Beryllium Copper Yes C17450 Profile Suppliers of C17450 C17455 Beryllium Copper Yes C17455 Profile Suppliers of C17455 C17460 * Beryllium Copper Yes C17460 Profile Suppliers of C17460 C17465 Beryllium Copper Yes C17465 Profile Suppliers of C17465 C17500 * Beryllium Copper Yes C17500 Profile Suppliers of C17500 C17510 * Beryllium Copper Yes C17510 Profile Suppliers of C17510 C17530 * Beryllium Copper Yes C17530 Profile Suppliers of C17530 C18090 Yes C18090 Profile Suppliers of C18090 C18160 Yes C18160 Profile Suppliers of C18160 C18670 MSP5 Yes C18670 Profile Suppliers of C18670 C19000 * Yes C19000 Profile Suppliers of C19000 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C40950 * Yes C40950 Profile Suppliers of C40950 C41125 * Yes C41125 Profile Suppliers of C41125 C42200 * Yes C42200 Profile Suppliers of C42200 C42210 * Tin Brass Yes C42210 Profile Suppliers of C42210 C42220 * Yes C42220 Profile Suppliers of C42220 C50580 * Yes C50580 Profile Suppliers of C50580 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51080 * Yes C51080 Profile Suppliers of C51080 C51100 * Yes C51100 Profile Suppliers of C51100 C51180 * Yes C51180 Profile Suppliers of C51180 C51980 * Yes C51980 Profile Suppliers of C51980 C63600 Yes C63600 Profile Suppliers of C63600 C68700 * Aluminum Brass, Arsenical Yes C68700 Profile Suppliers of C68700 C69150 * Copper Zinc Alloy (Copper Zinc Alloy) Yes C69150 Profile Suppliers of C69150 C72660 * Yes C72660 Profile Suppliers of C72660 C74500 * Nickel Silver, 65-10 Yes C74500 Profile Suppliers of C74500 C75200 * Nickel Silver, 65-18 Yes C75200 Profile Suppliers of C75200 C75400 Nickel Silver, 65-15 Yes C75400 Profile Suppliers of C75400 C75700 * Nickel Silver, 65-12 Yes C75700 Profile Suppliers of C75700 C76200 Nickel Silver Yes C76200 Profile Suppliers of C76200 C77100 Yes C77100 Profile Suppliers of C77100 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>