41 Alloys Found

Alloy UNS#DesignationActiveView

C15720 *

Dispersion Strengthned Alloy Yes C15720 Profile
Suppliers of C15720

C17000 *

Beryllium Copper Yes C17000 Profile
Suppliers of C17000

C17300

Beryllium Copper Yes C17300 Profile
Suppliers of C17300

C17400 *

Beryllium Copper No C17400 Profile
Suppliers of C17400

C17410 *

Beryllium Copper Yes C17410 Profile
Suppliers of C17410

C17500 *

Beryllium Copper Yes C17500 Profile
Suppliers of C17500

C17510 *

Beryllium Copper Yes C17510 Profile
Suppliers of C17510

C19000 *

Yes C19000 Profile
Suppliers of C19000

C19500 *

Yes C19500 Profile
Suppliers of C19500

C40810 *

Yes C40810 Profile
Suppliers of C40810

C40850 *

Yes C40850 Profile
Suppliers of C40850

C40860 *

Yes C40860 Profile
Suppliers of C40860

C42220 *

Yes C42220 Profile
Suppliers of C42220

C42520 *

Yes C42520 Profile
Suppliers of C42520

C42600 *

Yes C42600 Profile
Suppliers of C42600

C50780 *

Yes C50780 Profile
Suppliers of C50780

C51000 *

Phosphor Bronze, 5% A Yes C51000 Profile
Suppliers of C51000

C51080 *

Yes C51080 Profile
Suppliers of C51080

C51100 *

Yes C51100 Profile
Suppliers of C51100

C51180 *

Yes C51180 Profile
Suppliers of C51180

C51900 *

Yes C51900 Profile
Suppliers of C51900

C51980 *

Yes C51980 Profile
Suppliers of C51980

C63800 *

Yes C63800 Profile
Suppliers of C63800

C64740 *

Yes C64740 Profile
Suppliers of C64740

C64751

Yes C64751 Profile
Suppliers of C64751

C64760 *

Yes C64760 Profile
Suppliers of C64760

C64810

NKC4820 Yes C64810 Profile
Suppliers of C64810

C65400

Yes C65400 Profile
Suppliers of C65400

C66430 *

Yes C66430 Profile
Suppliers of C66430

C66700 *

Manganese Brass Yes C66700 Profile
Suppliers of C66700

C68800 *

Yes C68800 Profile
Suppliers of C68800

C69000 *

Copper Zinc No C69000 Profile
Suppliers of C69000

C69750

Yes C69750 Profile
Suppliers of C69750

C70265 *

Yes C70265 Profile
Suppliers of C70265

C70280 *

Yes C70280 Profile
Suppliers of C70280

C70290 *

Yes C70290 Profile
Suppliers of C70290

C70370 *

Yes C70370 Profile
Suppliers of C70370

C72500 *

Yes C72500 Profile
Suppliers of C72500

C72600 *

Copper Nickel No C72600 Profile
Suppliers of C72600

C72800 *

Yes C72800 Profile
Suppliers of C72800

C76200

Nickel Silver Yes C76200 Profile
Suppliers of C76200
* signifies an alloy registered with the U.S. EPA as Antimicrobial.