Saved Copper Alloys

Saved Searches

Copper Alloy Advanced Search Help

We'd Love Your Input

Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.

7 Alloys Found

Alloy UNS#DesignationActiveView

C35600

Extra High Leaded Brass Yes C35600 Profile
Suppliers of C35600

C38500

Architectural Bronze Yes C38500 Profile
Suppliers of C38500

C46750

Yes C46750 Profile
Suppliers of C46750

C48200

Naval Brass, Medium Leaded Yes C48200 Profile
Suppliers of C48200

C64200 *

Aluminum Bronze Yes C64200 Profile
Suppliers of C64200

C67400

Yes C67400 Profile
Suppliers of C67400

C67500

Manganese Bronze A Yes C67500 Profile
Suppliers of C67500
* signifies an alloy registered with the U.S. EPA as Antimicrobial.