3 Alloys Found

Alloy UNS#DesignationActiveView

C35600

Extra High Leaded Brass Yes C35600 Profile
Suppliers of C35600

C48200

Naval Brass, Medium Leaded Yes C48200 Profile
Suppliers of C48200

C48500

Naval Brass, High Leaded Yes C48500 Profile
Suppliers of C48500