3 Alloys Found

Alloy UNS#DesignationActiveView

C35350

Leaded Brass Yes C35350 Profile
Suppliers of C35350

C62400 *

Aluminum Bronze,11% Yes C62400 Profile
Suppliers of C62400

C63000 *

Aluminum Bronze Yes C63000 Profile
Suppliers of C63000