14 Alloys Found

Alloy UNS#DesignationActiveView

C28000 *

Muntz Metal, 60% Yes C28000 Profile
Suppliers of C28000

C28500

Copper-Zinc- Alloy (Brass) Yes C28500 Profile
Suppliers of C28500

C36500

Leaded Muntz Metal, Uninhibited Yes C36500 Profile
Suppliers of C36500

C36600

Leaded Muntz Metal, Arsinical No C36600 Profile
Suppliers of C36600

C36700

Leaded Muntz Metal, Antimonial No C36700 Profile
Suppliers of C36700

C36800

Leaded Brass No C36800 Profile
Suppliers of C36800

C37000

Free-Cutting Muntz Metal Yes C37000 Profile
Suppliers of C37000

C37100

Yes C37100 Profile
Suppliers of C37100

C46400

Naval Brass, Uninhibited Yes C46400 Profile
Suppliers of C46400

C46500

Naval Brass, Arsenical Yes C46500 Profile
Suppliers of C46500

C46600

Tin Brass No C46600 Profile
Suppliers of C46600

C46700

Tin Brass No C46700 Profile
Suppliers of C46700

C61900 *

Yes C61900 Profile
Suppliers of C61900

C68400 *

Yes C68400 Profile
Suppliers of C68400
* signifies an alloy registered with the U.S. EPA as Antimicrobial.