9 Alloys Found

Alloy UNS#DesignationActiveView

C83800

Hydraulic Bronze Yes C83800 Profile
Suppliers of C83800

C84030 *

Low Lead Semi-Red Brass Yes C84030 Profile
Suppliers of C84030

C84200

Yes C84200 Profile
Suppliers of C84200

C84400

Valve Metal Yes C84400 Profile
Suppliers of C84400

C85200

Leaded Yellow Brass Yes C85200 Profile
Suppliers of C85200

C87800 *

Cast Silicon Bronze Yes C87800 Profile
Suppliers of C87800

C87900

Copper Silicon Yes C87900 Profile
Suppliers of C87900

C90400 *

Tin Bronze Yes C90400 Profile
Suppliers of C90400

C90410 *

Tin Bronze Yes C90410 Profile
Suppliers of C90410