Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (4) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (3) You Searched For: coated-metal-arc-welding:"Poor" gas-shielded-arc-welding:"Fair" CLEAR this search X SAVE this search << Page 1 >> 4 Alloys Found Alloy UNS#DesignationActiveView C14750 * High Copper Alloy Yes C14750 Profile Suppliers of C14750 C53400 Phosphor Bronze B-1 Yes C53400 Profile Suppliers of C53400 C68350 * Low Silicon Brass Yes C68350 Profile Suppliers of C68350 C85550 * Low Silicon Brass Yes C85550 Profile Suppliers of C85550 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>