28 Alloys Found

Alloy UNS#DesignationActiveView

C11000 *

Electrolytic Tough Pitch (ETP) Yes C11000 Profile
Suppliers of C11000

C11100 *

Electronic Tough Pitch, Anneal Resistant (ETP) Yes C11100 Profile
Suppliers of C11100

C11300 *

Tough Pitch with Ag (STP) Yes C11300 Profile
Suppliers of C11300

C11400 *

Tough Pitch with Ag (STP) Yes C11400 Profile
Suppliers of C11400

C11500 *

Tough Pitch with Ag (STP) Yes C11500 Profile
Suppliers of C11500

C11600 *

Tough Pitch with Ag (STP) Yes C11600 Profile
Suppliers of C11600

C12500 *

Fire-Refined Tough Pitch (FRTP) Yes C12500 Profile
Suppliers of C12500

C12510 *

Yes C12510 Profile
Suppliers of C12510

C12700 *

Copper Alloy No C12700 Profile
Suppliers of C12700

C12800 *

Copper Alloy No C12800 Profile
Suppliers of C12800

C12900 *

Fire-Refined Tough Pitch with Ag (FRSTP) Yes C12900 Profile
Suppliers of C12900

C13000

Copper Alloy No C13000 Profile
Suppliers of C13000

C13150 *

Copper Yes C13150 Profile
Suppliers of C13150

C14500 *

Tellurium-Bearing (PTE) Yes C14500 Profile
Suppliers of C14500

C14510 *

Tellurium-Bearing Yes C14510 Profile
Suppliers of C14510

C14520 *

Phosphorus-Deoxidized,Tellurium-Bearing (DPTE) Yes C14520 Profile
Suppliers of C14520

C14750 *

High Copper Alloy Yes C14750 Profile
Suppliers of C14750

C15000 *

Zirconium Copper Yes C15000 Profile
Suppliers of C15000

C15100 *

Yes C15100 Profile
Suppliers of C15100

C15630

Yes C15630 Profile
Suppliers of C15630

C15715 *

Dispersion Strengthened Alloy Yes C15715 Profile
Suppliers of C15715

C15720 *

Dispersion Strengthned Alloy Yes C15720 Profile
Suppliers of C15720

C15730 *

Copper Alloy Yes C15730 Profile
Suppliers of C15730

C15750 *

Dispersion Strengthened Copper (C3/60) Yes C15750 Profile
Suppliers of C15750

C15760 *

Dispersion Strengthened Alloy Yes C15760 Profile
Suppliers of C15760

C15780 *

Copper Alloy Yes C15780 Profile
Suppliers of C15780

C15790 *

Copper Alloy Yes C15790 Profile
Suppliers of C15790

C15900 *

Dispersion Strengthened Coper (C3/11) Yes C15900 Profile
Suppliers of C15900
* signifies an alloy registered with the U.S. EPA as Antimicrobial.