Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (4) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (4) You Searched For: copper-alloy_metadata_alloy-type:"Wrought" copper-alloy_metadata_alloy-class:"HIGH COPPER ALLOYS" rockwell-30t-scale:[65 TO 70] CLEAR this search X SAVE this search << Page 1 >> 4 Alloys Found Alloy UNS#DesignationActiveView C16500 * Yes C16500 Profile Suppliers of C16500 C17000 * Beryllium Copper Yes C17000 Profile Suppliers of C17000 C17200 * Beryllium Copper Yes C17200 Profile Suppliers of C17200 C19400 * Yes C19400 Profile Suppliers of C19400 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>