6 Alloys Found

Alloy UNS#DesignationActiveView

C17200 *

Beryllium Copper Yes C17200 Profile
Suppliers of C17200

C61000 *

Yes C61000 Profile
Suppliers of C61000

C61300 *

Yes C61300 Profile
Suppliers of C61300

C61400 *

Yes C61400 Profile
Suppliers of C61400

C64400 *

Aluminum Bronze No C64400 Profile
Suppliers of C64400

C99750

Yes C99750 Profile
Suppliers of C99750