6 Alloys Found

Alloy UNS#DesignationActiveView

C19200 *

Yes C19200 Profile
Suppliers of C19200

C64800 *

NKC4419 Yes C64800 Profile
Suppliers of C64800

C64810

NKC4820 Yes C64810 Profile
Suppliers of C64810

C64850

Yes C64850 Profile
Suppliers of C64850

C81300 *

Copper Alloy No C81300 Profile
Suppliers of C81300

C81400

Beryllium Copper 70C Yes C81400 Profile
Suppliers of C81400
* signifies an alloy registered with the U.S. EPA as Antimicrobial.