3 Alloys Found

Alloy UNS#DesignationActiveView

C19200 *

Yes C19200 Profile
Suppliers of C19200

C19710 *

Yes C19710 Profile
Suppliers of C19710

C64800 *

NKC4419 Yes C64800 Profile
Suppliers of C64800
* signifies an alloy registered with the U.S. EPA as Antimicrobial.