38 Alloys Found

Alloy UNS#DesignationActiveView

C89320 *

Yes C89320 Profile
Suppliers of C89320

C89833 *

Copper Bismuth Alloy Yes C89833 Profile
Suppliers of C89833

C89836

Copper Bismuth Alloy Yes C89836 Profile
Suppliers of C89836

C89844

Yes C89844 Profile
Suppliers of C89844

C90200

Yes C90200 Profile
Suppliers of C90200

C90300

Tin Bronze Yes C90300 Profile
Suppliers of C90300

C90400 *

Tin Bronze Yes C90400 Profile
Suppliers of C90400

C92200

Navy M Bronze Yes C92200 Profile
Suppliers of C92200

C92600

Yes C92600 Profile
Suppliers of C92600

C15715 *

Dispersion Strengthened Alloy Yes C15715 Profile
Suppliers of C15715

C17500 *

Beryllium Copper Yes C17500 Profile
Suppliers of C17500

C17510 *

Beryllium Copper Yes C17510 Profile
Suppliers of C17510

C19200 *

Yes C19200 Profile
Suppliers of C19200

C22000 *

Commercial Bronze, 90% Yes C22000 Profile
Suppliers of C22000

C23000 *

Red Brass, 85% Yes C23000 Profile
Suppliers of C23000

C24000 *

Low Brass, 80% Yes C24000 Profile
Suppliers of C24000

C27453

Copper Zinc Alloy Yes C27453 Profile
Suppliers of C27453

C40500 *

Penny Bronze Yes C40500 Profile
Suppliers of C40500

C41300 *

Tin Brass Yes C41300 Profile
Suppliers of C41300

C41500 *

Tin Brass Yes C41500 Profile
Suppliers of C41500

C42200 *

Yes C42200 Profile
Suppliers of C42200

C43400 *

Yes C43400 Profile
Suppliers of C43400

C46750

Yes C46750 Profile
Suppliers of C46750

C51000 *

Phosphor Bronze, 5% A Yes C51000 Profile
Suppliers of C51000

C51080 *

Yes C51080 Profile
Suppliers of C51080

C51100 *

Yes C51100 Profile
Suppliers of C51100

C51180 *

Yes C51180 Profile
Suppliers of C51180

C51900 *

Yes C51900 Profile
Suppliers of C51900

C51980 *

Yes C51980 Profile
Suppliers of C51980

C52180 *

Yes C52180 Profile
Suppliers of C52180

C52480 *

Yes C52480 Profile
Suppliers of C52480

C65100 *

Low-Silicon Bronze B Yes C65100 Profile
Suppliers of C65100

C75400

Nickel Silver, 65-15 Yes C75400 Profile
Suppliers of C75400

C82200 *

Beryllium Copper 30C Yes C82200 Profile
Suppliers of C82200

C83400

Yes C83400 Profile
Suppliers of C83400

C83600

Ounce Metal Yes C83600 Profile
Suppliers of C83600

C84200

Yes C84200 Profile
Suppliers of C84200

C84500

Yes C84500 Profile
Suppliers of C84500
* signifies an alloy registered with the U.S. EPA as Antimicrobial.