Saved Copper Alloys

Saved Searches

Copper Alloy Advanced Search Help

We'd Love Your Input

Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.

35 Alloys Found

Alloy UNS#DesignationActiveView

C18670

MSP5 Yes C18670 Profile
Suppliers of C18670

C27450

Yellow Brass Yes C27450 Profile
Suppliers of C27450

C40500 *

Penny Bronze Yes C40500 Profile
Suppliers of C40500

C40950 *

Yes C40950 Profile
Suppliers of C40950

C41100 *

Tin Brass Yes C41100 Profile
Suppliers of C41100

C41120 *

Yes C41120 Profile
Suppliers of C41120

C41125 *

Yes C41125 Profile
Suppliers of C41125

C42230

Yes C42230 Profile
Suppliers of C42230

C46750

Yes C46750 Profile
Suppliers of C46750

C50780 *

Yes C50780 Profile
Suppliers of C50780

C51000 *

Phosphor Bronze, 5% A Yes C51000 Profile
Suppliers of C51000

C51080 *

Yes C51080 Profile
Suppliers of C51080

C51100 *

Yes C51100 Profile
Suppliers of C51100

C51180 *

Yes C51180 Profile
Suppliers of C51180

C51900 *

Yes C51900 Profile
Suppliers of C51900

C51980 *

Yes C51980 Profile
Suppliers of C51980

C52100 *

Phospher Bronze, 8% C Yes C52100 Profile
Suppliers of C52100

C52180 *

Yes C52180 Profile
Suppliers of C52180

C52400 *

Phospher Bronze 10% D Yes C52400 Profile
Suppliers of C52400

C52480 *

Yes C52480 Profile
Suppliers of C52480

C53800

Yes C53800 Profile
Suppliers of C53800

C64725 *

Copper Silicon Alloy Yes C64725 Profile
Suppliers of C64725

C64727 *

Copper Silicon Alloy (MAX375) Yes C64727 Profile
Suppliers of C64727

C69150 *

Copper Zinc Alloy (Copper Zinc Alloy) Yes C69150 Profile
Suppliers of C69150

C69750

Yes C69750 Profile
Suppliers of C69750

C70290 *

Yes C70290 Profile
Suppliers of C70290

C83400

Yes C83400 Profile
Suppliers of C83400

C83450

Yes C83450 Profile
Suppliers of C83450

C90200

Yes C90200 Profile
Suppliers of C90200

C90300

Tin Bronze Yes C90300 Profile
Suppliers of C90300

C90500

Gun Metal Yes C90500 Profile
Suppliers of C90500

C90700

Tin Bronze, 65 Yes C90700 Profile
Suppliers of C90700

C91600

Yes C91600 Profile
Suppliers of C91600

C91700

Nickel Gear Bronze Yes C91700 Profile
Suppliers of C91700

C94700 *

Cast Nickel-Tin Bronze Yes C94700 Profile
Suppliers of C94700
* signifies an alloy registered with the U.S. EPA as Antimicrobial.