133 Alloys Found

Alloy UNS#DesignationActiveView

C10100 *

Oxygen-Free-Electronic (OFE) Yes C10100 Profile
Suppliers of C10100

C12510 *

Yes C12510 Profile
Suppliers of C12510

C15710 *

Copper Alloy No C15710 Profile
Suppliers of C15710

C15720 *

Dispersion Strengthned Alloy Yes C15720 Profile
Suppliers of C15720

C15735 *

Copper Alloy No C15735 Profile
Suppliers of C15735

C15760 *

Dispersion Strengthened Alloy Yes C15760 Profile
Suppliers of C15760

C16200 *

Cadmium Copper Yes C16200 Profile
Suppliers of C16200

C16500 *

Yes C16500 Profile
Suppliers of C16500

C17400 *

Beryllium Copper No C17400 Profile
Suppliers of C17400

C17410 *

Beryllium Copper Yes C17410 Profile
Suppliers of C17410

C17450 *

Beryllium Copper Yes C17450 Profile
Suppliers of C17450

C17460 *

Beryllium Copper Yes C17460 Profile
Suppliers of C17460

C17500 *

Beryllium Copper Yes C17500 Profile
Suppliers of C17500

C17510 *

Beryllium Copper Yes C17510 Profile
Suppliers of C17510

C18200

Chromium Copper Yes C18200 Profile
Suppliers of C18200

C18400

Chromium Copper Yes C18400 Profile
Suppliers of C18400

C19000 *

Yes C19000 Profile
Suppliers of C19000

C19100

Yes C19100 Profile
Suppliers of C19100

C19140

Yes C19140 Profile
Suppliers of C19140

C19160

Yes C19160 Profile
Suppliers of C19160

C19210 *

Yes C19210 Profile
Suppliers of C19210

C19220 *

Yes C19220 Profile
Suppliers of C19220

C19280 *

Yes C19280 Profile
Suppliers of C19280

C19419 *

CAC19 (High Copper) Yes C19419 Profile
Suppliers of C19419

C19500 *

Yes C19500 Profile
Suppliers of C19500

C19800 *

Yes C19800 Profile
Suppliers of C19800

C19810 *

Hig Copper Alloy Yes C19810 Profile
Suppliers of C19810

C19910 *

NKT 322 (High Copper) Yes C19910 Profile
Suppliers of C19910

C21000 *

Gilding, 95% Yes C21000 Profile
Suppliers of C21000

C22000 *

Commercial Bronze, 90% Yes C22000 Profile
Suppliers of C22000

C22600 *

Jewelry Bronze, 87-1/2% Yes C22600 Profile
Suppliers of C22600

C23000 *

Red Brass, 85% Yes C23000 Profile
Suppliers of C23000

C24000 *

Low Brass, 80% Yes C24000 Profile
Suppliers of C24000

C26800 *

Yellow Brass, 66% Yes C26800 Profile
Suppliers of C26800

C27000 *

Yellow Brass, 65% Yes C27000 Profile
Suppliers of C27000

C31400

Leaded Commercial Bronze Yes C31400 Profile
Suppliers of C31400

C31600

Leaded Commercial Bronze (Nickel-Bearing) Yes C31600 Profile
Suppliers of C31600

C33500

Low-Leaded Brass Yes C33500 Profile
Suppliers of C33500

C34000

Medium Leaded Brass, 64-1/2% Yes C34000 Profile
Suppliers of C34000

C34500

Yes C34500 Profile
Suppliers of C34500

C35000

Medium Leaded Brass, 62% Yes C35000 Profile
Suppliers of C35000

C35300

High Leaded Brass, 62% Yes C35300 Profile
Suppliers of C35300

C35600

Extra High Leaded Brass Yes C35600 Profile
Suppliers of C35600

C36000

Free-Cutting Brass Yes C36000 Profile
Suppliers of C36000

C36010

Leaded Brass (Free-Cutting Brass) Yes C36010 Profile
Suppliers of C36010

C40500 *

Penny Bronze Yes C40500 Profile
Suppliers of C40500

C40800 *

Silicon Brass No C40800 Profile
Suppliers of C40800

C40810 *

Yes C40810 Profile
Suppliers of C40810

C40850 *

Yes C40850 Profile
Suppliers of C40850

C40860 *

Yes C40860 Profile
Suppliers of C40860
* signifies an alloy registered with the U.S. EPA as Antimicrobial.