8 Alloys Found

Alloy UNS#DesignationActiveView

C42200 *

Yes C42200 Profile
Suppliers of C42200

C61900 *

Yes C61900 Profile
Suppliers of C61900

C62300 *

Aluminum Bronze, 9% Yes C62300 Profile
Suppliers of C62300

C64200 *

Aluminum Bronze Yes C64200 Profile
Suppliers of C64200

C64400 *

Aluminum Bronze No C64400 Profile
Suppliers of C64400

C86500

Manganese Bronze Yes C86500 Profile
Suppliers of C86500

C87200

Silicon Bronze No C87200 Profile
Suppliers of C87200

C87400

Yes C87400 Profile
Suppliers of C87400
* signifies an alloy registered with the U.S. EPA as Antimicrobial.