Saved Copper Alloys

Saved Searches

Copper Alloy Advanced Search Help

We'd Love Your Input

Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.

10 Alloys Found

Alloy UNS#DesignationActiveView

C22600 *

Jewelry Bronze, 87-1/2% Yes C22600 Profile
Suppliers of C22600

C34200

High Leaded Brass, 64-1/2% Yes C34200 Profile
Suppliers of C34200

C35300

High Leaded Brass, 62% Yes C35300 Profile
Suppliers of C35300

C51100 *

Yes C51100 Profile
Suppliers of C51100

C52100 *

Phospher Bronze, 8% C Yes C52100 Profile
Suppliers of C52100

C63800 *

Yes C63800 Profile
Suppliers of C63800

C64400 *

Aluminum Bronze No C64400 Profile
Suppliers of C64400

C68800 *

Yes C68800 Profile
Suppliers of C68800

C72650 *

Yes C72650 Profile
Suppliers of C72650

C74500 *

Nickel Silver, 65-10 Yes C74500 Profile
Suppliers of C74500