3 Alloys Found

Alloy UNS#DesignationActiveView

C51100 *

Yes C51100 Profile
Suppliers of C51100

C52100 *

Phospher Bronze, 8% C Yes C52100 Profile
Suppliers of C52100

C74500 *

Nickel Silver, 65-10 Yes C74500 Profile
Suppliers of C74500
* signifies an alloy registered with the U.S. EPA as Antimicrobial.