Saved Copper Alloys

Saved Searches

Copper Alloy Advanced Search Help

We'd Love Your Input

Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.

3 Alloys Found

Alloy UNS#DesignationActiveView

C74500 *

Nickel Silver, 65-10 Yes C74500 Profile
Suppliers of C74500

C75200 *

Nickel Silver, 65-18 Yes C75200 Profile
Suppliers of C75200

C76390

Copper Nickel Zinc No C76390 Profile
Suppliers of C76390
* signifies an alloy registered with the U.S. EPA as Antimicrobial.