10 Alloys Found

Alloy UNS#DesignationActiveView

C15000 *

Zirconium Copper Yes C15000 Profile
Suppliers of C15000

C16500 *

Yes C16500 Profile
Suppliers of C16500

C34000

Medium Leaded Brass, 64-1/2% Yes C34000 Profile
Suppliers of C34000

C34200

High Leaded Brass, 64-1/2% Yes C34200 Profile
Suppliers of C34200

C35000

Medium Leaded Brass, 62% Yes C35000 Profile
Suppliers of C35000

C35300

High Leaded Brass, 62% Yes C35300 Profile
Suppliers of C35300

C36000

Free-Cutting Brass Yes C36000 Profile
Suppliers of C36000

C36010

Leaded Brass (Free-Cutting Brass) Yes C36010 Profile
Suppliers of C36010

C36200

Leaded Brass No C36200 Profile
Suppliers of C36200

C63600

Yes C63600 Profile
Suppliers of C63600