Saved Copper Alloys

Saved Searches

Copper Alloy Advanced Search Help

We'd Love Your Input

Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.

35 Alloys Found

Alloy UNS#DesignationActiveView

C18200

Chromium Copper Yes C18200 Profile
Suppliers of C18200

C18400

Chromium Copper Yes C18400 Profile
Suppliers of C18400

C18500

High Copper No C18500 Profile
Suppliers of C18500

C19000 *

Yes C19000 Profile
Suppliers of C19000

C23000 *

Red Brass, 85% Yes C23000 Profile
Suppliers of C23000

C24000 *

Low Brass, 80% Yes C24000 Profile
Suppliers of C24000

C26000 *

Cartridge Brass, 70% Yes C26000 Profile
Suppliers of C26000

C26100 *

Brass No C26100 Profile
Suppliers of C26100

C26130 *

Yes C26130 Profile
Suppliers of C26130

C26200 *

Yes C26200 Profile
Suppliers of C26200

C26800 *

Yellow Brass, 66% Yes C26800 Profile
Suppliers of C26800

C27000 *

Yellow Brass, 65% Yes C27000 Profile
Suppliers of C27000

C27400 *

Yellow Brass, 63% Yes C27400 Profile
Suppliers of C27400

C28000 *

Muntz Metal, 60% Yes C28000 Profile
Suppliers of C28000

C33000

Low Leaded Brass (Tube) Yes C33000 Profile
Suppliers of C33000

C33100

Leaded Brass No C33100 Profile
Suppliers of C33100

C33200

High Leaded Brass (Tube) Yes C33200 Profile
Suppliers of C33200

C34000

Medium Leaded Brass, 64-1/2% Yes C34000 Profile
Suppliers of C34000

C35000

Medium Leaded Brass, 62% Yes C35000 Profile
Suppliers of C35000

C35600

Extra High Leaded Brass Yes C35600 Profile
Suppliers of C35600

C36000

Free-Cutting Brass Yes C36000 Profile
Suppliers of C36000

C36010

Leaded Brass (Free-Cutting Brass) Yes C36010 Profile
Suppliers of C36010

C40500 *

Penny Bronze Yes C40500 Profile
Suppliers of C40500

C42500 *

Yes C42500 Profile
Suppliers of C42500

C43400 *

Yes C43400 Profile
Suppliers of C43400

C46400

Naval Brass, Uninhibited Yes C46400 Profile
Suppliers of C46400

C46500

Naval Brass, Arsenical Yes C46500 Profile
Suppliers of C46500

C46600

Tin Brass No C46600 Profile
Suppliers of C46600

C46700

Tin Brass No C46700 Profile
Suppliers of C46700

C51000 *

Phosphor Bronze, 5% A Yes C51000 Profile
Suppliers of C51000

C51100 *

Yes C51100 Profile
Suppliers of C51100

C54400

Phosphor Bronze B-2 Yes C54400 Profile
Suppliers of C54400

C65100 *

Low-Silicon Bronze B Yes C65100 Profile
Suppliers of C65100

C74500 *

Nickel Silver, 65-10 Yes C74500 Profile
Suppliers of C74500

C75700 *

Nickel Silver, 65-12 Yes C75700 Profile
Suppliers of C75700
* signifies an alloy registered with the U.S. EPA as Antimicrobial.