80 Alloys Found

Alloy UNS#DesignationActiveView

C15500 *

Yes C15500 Profile
Suppliers of C15500

C15760 *

Dispersion Strengthened Alloy Yes C15760 Profile
Suppliers of C15760

C17000 *

Beryllium Copper Yes C17000 Profile
Suppliers of C17000

C17200 *

Beryllium Copper Yes C17200 Profile
Suppliers of C17200

C17500 *

Beryllium Copper Yes C17500 Profile
Suppliers of C17500

C17510 *

Beryllium Copper Yes C17510 Profile
Suppliers of C17510

C18100

Yes C18100 Profile
Suppliers of C18100

C18150

Yes C18150 Profile
Suppliers of C18150

C18200

Chromium Copper Yes C18200 Profile
Suppliers of C18200

C18400

Chromium Copper Yes C18400 Profile
Suppliers of C18400

C18500

High Copper No C18500 Profile
Suppliers of C18500

C19000 *

Yes C19000 Profile
Suppliers of C19000

C22600 *

Jewelry Bronze, 87-1/2% Yes C22600 Profile
Suppliers of C22600

C23000 *

Red Brass, 85% Yes C23000 Profile
Suppliers of C23000

C24000 *

Low Brass, 80% Yes C24000 Profile
Suppliers of C24000

C26000 *

Cartridge Brass, 70% Yes C26000 Profile
Suppliers of C26000

C26100 *

Brass No C26100 Profile
Suppliers of C26100

C26130 *

Yes C26130 Profile
Suppliers of C26130

C26200 *

Yes C26200 Profile
Suppliers of C26200

C26800 *

Yellow Brass, 66% Yes C26800 Profile
Suppliers of C26800

C27000 *

Yellow Brass, 65% Yes C27000 Profile
Suppliers of C27000

C28000 *

Muntz Metal, 60% Yes C28000 Profile
Suppliers of C28000

C33200

High Leaded Brass (Tube) Yes C33200 Profile
Suppliers of C33200

C33500

Low-Leaded Brass Yes C33500 Profile
Suppliers of C33500

C34000

Medium Leaded Brass, 64-1/2% Yes C34000 Profile
Suppliers of C34000

C34200

High Leaded Brass, 64-1/2% Yes C34200 Profile
Suppliers of C34200

C34500

Yes C34500 Profile
Suppliers of C34500

C35000

Medium Leaded Brass, 62% Yes C35000 Profile
Suppliers of C35000

C35300

High Leaded Brass, 62% Yes C35300 Profile
Suppliers of C35300

C35600

Extra High Leaded Brass Yes C35600 Profile
Suppliers of C35600

C36000

Free-Cutting Brass Yes C36000 Profile
Suppliers of C36000

C36010

Leaded Brass (Free-Cutting Brass) Yes C36010 Profile
Suppliers of C36010

C36200

Leaded Brass No C36200 Profile
Suppliers of C36200

C37000

Free-Cutting Muntz Metal Yes C37000 Profile
Suppliers of C37000

C37100

Yes C37100 Profile
Suppliers of C37100

C40500 *

Penny Bronze Yes C40500 Profile
Suppliers of C40500

C40800 *

Silicon Brass No C40800 Profile
Suppliers of C40800

C41100 *

Tin Brass Yes C41100 Profile
Suppliers of C41100

C41300 *

Tin Brass Yes C41300 Profile
Suppliers of C41300

C41500 *

Tin Brass Yes C41500 Profile
Suppliers of C41500

C42200 *

Yes C42200 Profile
Suppliers of C42200

C42500 *

Yes C42500 Profile
Suppliers of C42500

C43000 *

Tin Brass Yes C43000 Profile
Suppliers of C43000

C43400 *

Yes C43400 Profile
Suppliers of C43400

C43500 *

Tin Brass Yes C43500 Profile
Suppliers of C43500

C46400

Naval Brass, Uninhibited Yes C46400 Profile
Suppliers of C46400

C46500

Naval Brass, Arsenical Yes C46500 Profile
Suppliers of C46500

C46600

Tin Brass No C46600 Profile
Suppliers of C46600

C46700

Tin Brass No C46700 Profile
Suppliers of C46700

C48500

Naval Brass, High Leaded Yes C48500 Profile
Suppliers of C48500
* signifies an alloy registered with the U.S. EPA as Antimicrobial.